Dry strength agents are polymeric paper additives used to improve strength measured after a sheet is dried and conditioned. The category includes several chemistries, charge types and molecular architectures. The Rriver Chemical listing references CAS 9003-05-8, which identifies polyacrylamide (PAM), but that CAS number alone does not define ionic charge, copolymer composition, molecular weight or application performance.
For Rriver Chemical supply information, see the Dry Strength Agent product page.
Identity is more than a generic product name
PubChem associates CAS 9003-05-8 with polyacrylamide and gives the repeating formula as (C3H5NO)x. Commercial paper dry strength products may be cationic, anionic, amphoteric, glyoxalated or otherwise modified; their composition and use cannot be inferred from the base-polymer CAS number. Source: PubChem, Polyacrylamide.
The purchase specification should name the product grade and form, ionic character, active content and intended paper application. The quotation, COA, SDS, package label and shipment documents should identify the same manufacturer, factory and batch.
How dry strength programs support paper performance
Fiber bonding and sheet structure
Dry strength depends on fiber quality, refining, bonded area, sheet formation, moisture and multiple wet-end interactions. A properly selected polymer can support inter-fiber bonding and help a mill reach tensile, burst, compression or internal-bond targets. It cannot restore every property lost through poor formation, unsuitable furnish or an unstable process.
Kemira states that many of its dry strength products are cationic or anionic polymers based on polyacrylamide chemistry and can be added at the wet end or by sheet spray. Solenis lists amphoteric polyacrylamide among its dry-strength technologies. These examples demonstrate that “PAM” covers multiple functional designs rather than one interchangeable commodity. Source: Kemira, Dry Strength Additives; Source: Solenis, Strength Additives.
Charge and furnish compatibility
Polymer charge affects adsorption, retention and interaction with fibers, fines, fillers and other additives. Furnish changes, conductivity, pH, dissolved and colloidal substances, charge demand and addition sequence can change the response. Buyers should obtain charge-type and charge-density information suitable for their control strategy and confirm it through laboratory and machine trials.
Dry strength is not wet strength
Dry strength tests are performed after paper has dried and been conditioned. Wet strength concerns resistance after wetting and commonly uses different resin technologies. Some chemistries can influence both, but a product should not be described as wet-strength resin unless its formulation, intended use and performance data support that claim.
Specifications that matter
Depending on whether the product is a solution, emulsion or powder, a specification may address active solids, viscosity, pH, density, ionic character, charge density, molecular-weight range, residual monomer, color and storage stability. The exact limits and methods must be agreed for the supplied grade.
- Product identity: record the grade, polymer family, charge type and physical form.
- Concentration: define active solids or active polymer, basis, tolerance and method.
- Application properties: agree viscosity and dilution behavior under stated test conditions.
- Controlled residuals: set relevant impurity limits and reporting thresholds from the risk assessment.
- Traceability: require lot-specific COA, label, SDS and manufacturing-site information.
TAPPI’s wet-end chemistry reference separates cationic, anionic, amphoteric and glyoxalated polyacrylamide technologies and emphasizes application optimization, addition-point selection, metering, dilution and paper testing. This reinforces the need to evaluate the complete program rather than compare products by CAS number or solids alone. Source: TAPPI, Advances in Papermaking Wet End Chemistry.
Plan a controlled product trial
Define the target and baseline
Choose the target paper grade and performance metrics before the trial. Common measures can include tensile strength, tensile energy absorption, burst, ring crush, short-span compression, internal bond, folding endurance, drainage, retention, formation and machine speed. Use test methods appropriate to the grade and compare against a stable baseline.
Control dose and addition point
Prepare the product using the supplier’s documented dilution and aging procedure. Record water quality, mixing energy, solution age, dose, addition point and contact time. Polymer overfeed can be uneconomic and may disturb formation, drainage, deposits or system charge, so the trial should cover a controlled dose range.
Evaluate economics on finished performance
Cost per tonne of product is not the same as cost per tonne of paper. Calculate delivered active polymer, achieved strength, fiber or basis-weight opportunity, machine productivity and any effect on other additives. Verify results over enough production to separate the treatment effect from normal furnish and machine variation.
Packaging, storage and receiving

The photograph does not prove current inventory, product identity or packaging availability. Request the current SDS and storage statement for the exact grade. Define drum, IBC, bag or bulk packaging, seal, net weight, palletization and label fields. Receiving checks should reconcile the lot, COA and package before sampling under an approved procedure.
Polymer products can be sensitive to temperature, freezing, contamination, shear or storage time. Follow the manufacturer-specific shelf life and handling limits. Spilled polymer solutions may create very slippery surfaces, so the site should maintain an appropriate containment and cleanup procedure.
Price and quotation comparison
Compare dry strength agent price on the same polymer family, charge, active-content basis, quantity, packaging, Incoterm, destination and service scope. Ask a manufacturer, factory, exporter or supplier to state quotation validity, lead time and available specification, COA, SDS and trial support. A dilute or poorly matched product can be more expensive even when its price per tonne is lower.
Frequently asked questions
Does CAS 9003-05-8 define a complete dry strength grade?
No. It identifies polyacrylamide generally, while charge, copolymer composition, molecular architecture, concentration and physical form still require specification.
Will a higher dosage always give higher paper strength?
No. Response depends on adsorption, furnish and process conditions, and excessive dose can reduce efficiency or disrupt other wet-end functions.
What should an inquiry include?
State furnish and paper grade, target strength tests, current wet-end conditions, desired product form, quantity, package, destination and required specification, COA and SDS.
Request dry strength agent documentation
Explore Rriver Chemical’s Paper Making Chemicals, or contact Rriver Chemical to request available Dry Strength Agent documentation and a quotation. Final compatibility, dosage and performance must be established for the exact grade through controlled mill trials.
References checked on September 16, 2026. This article provides general procurement information and does not replace the current supplier specification, safety data sheet, process review or mill trial.